Electrodeposited coating
Electrodeposited coating with an inorganic/organic leachant/sealant
Designation: NEN - EN 12329-Fe/Zn8/A/T2
Layer thickness: 8-12 µm
Corrosion resistance: Minimum 96 hours neutral salt spray (ISO-9227/ ASTM- B 117) before zinc corrosion (white) occurs. And 500 hours to the first signs of red rust.
Go back to previous page
Designation: NEN - EN 12329-Fe/Zn8/A/T2
Layer thickness: 8-12 µm
Corrosion resistance: Minimum 96 hours neutral salt spray (ISO-9227/ ASTM- B 117) before zinc corrosion (white) occurs. And 500 hours to the first signs of red rust.